MEW MARTIAN
Description
Multilayer PVD coating 2.5 microns thick. It is obtained from plasma with a specific titanium, carbon and acetylene composition; this gives the coating a very low friction coefficient of 0.18 as well as a considerable deposited-layer hardness of 3.200 Vickers (HV 0.05). read moreDescription
Multilayer PVD coating 2.5 microns thick. It is obtained from plasma with a specific titanium, carbon and acetylene composition; this gives the coating a very low friction coefficient of 0.18 as well as a considerable deposited-layer hardness of 3.200 Vickers (HV 0.05).
It is particularly suitable for cutting stainless steel, titanium, hardened steel as well as brass and copper.
Coating Features
Suitable for cutting | Medium-alloy steel 700 – 900 N/mm2, Titanium, Copper, Bronze, Brass, Aluminium (With Lubrication) |
Steel friction coefficient(dry) | 0.18 |
Thickness | 2.5 |
Maximum Working Temperature | 450°C |
Deposition temperature | 480°C |
Coefficient of thermal expansion (10-6/°K) | 10 |
Micro-Hardness HV (0,05) | 3200 |